:focal(undefined))
β-TCP Compound Powder Our β-TCP Compound Powder is created through spray drying, resulting in particle sizes primarily ranging from 20 to 60 µm. Its highly porous surface makes it ideal for processing with polymers, particularly in the production of medical implant composites such as bone screws, interference screws, and suture anchors. Milled β-TCP Powder The Milled β-TCP Powder is a highly pure form of β-TCP, milled to achieve a mean particle size of less than 5 µm. With a narrow particle size distribution, it contains no particles larger than 10 µm, ensuring a clean cut-off that eliminates concerns about nano-sized particles. The powder’s good particle roundness enhances its versatility and usability, making it a superior choice for diverse medical application